Atactic Polymer |
C∞1 |
Bisphenol A Polysulfone |
2.2 |
Poly(Bisphenol A carbonate) |
2.4 |
Poly(Bisphenol A terephthalate) |
2.6 |
Poly(2,6-dimethyl-p-phenylene oxide),
PPO |
3.0 |
Poly(tetramethyl Bisphenol A carbonate) |
3.1 |
Poly(bisphenol A isophthalate) |
3.7 |
Poly(ethylene terephthalate), PET |
4.1 |
Bisphenol-A diglycidyl ether epoxy resin |
4.7 |
Poly(1,4-butadiene) |
5.3 |
Poly(1-butene), PB-1 |
5.8 |
Poly(propylene), PP |
6.0 |
Poly(caprolactam), Nylon 6 |
6.2 |
Poly(hexamethylene adipamide), Nylon 6,6 |
6.5 |
Poly(isobutene), PIB |
6.7 |
Poly(ethylene glycol), PEG |
6.9 |
Poly(ethylene), PE |
6.9 |
PoIy(1,2-butadiene) |
7.4 |
Polyacetal, POM |
7.5 |
Poly(vinyl chloride), PVC |
7.6 |
Poly(ethyl methacrylate) |
8.0 |
Poly(methyl acrylate), PMA |
8.1 |
Poly(methyl methacrylate), PMMA |
8.1 |
Poly(ethyl acrylate), PEA |
9.3 |
Poly(vinyl acetate) |
9.4 |
Poly(α-methylstyrene) |
10.1 |
Polystyrene |
10.3 |
Poly(octyl methacrylate), POMA |
12.1 |
Poly(hexyl methacrylate) |
12.2 |
Poly(acrylamide) |
12.7 |
Poly(dodecyl methacrylate) |
14.1 |
Poly(octadecyl methacrylate) |
20.6 |